Nov 25, 2016

Compound after the film to compound, and some orange peel surface appears, the main reason for this is it?

After one, because the powder, curing at high temperature processing, small deformation of powder heating and pressure, composite film formation of orange peel surface;

Second, because composite anti-static films immediately after the curing process, rapid precipitation by the adhesive layer of anti-static agent, and orange peel surface.

Solution methods are:

Without powder coating, curing temperature should be lowered to below 40 degrees, reducing rolling pressure;

Second, the composite curing process fee for a period of time and then after, improve the grade of anti-static film.